Desizing Starch Sized Fabric

Desizing Starch-Sized Fabric: Why Residual Size Ruins Dyeing, and How to Check It

By the Shalbond Technical Team · Updated November 2026

The short answer

Warp size protects yarn on the loom, but it must come out before bleaching, dyeing or printing. Residual size “resist[s] dyes and chemicals” [1]. The starch technology literature notes that residual sizing agents “make it impossible to obtain a well-penetrated and evenly-dyed material” [2, p. 331].

For starch sizes, enzymatic desizing is the most common method on cotton. It breaks starch into soluble fragments without damaging the fibre [1][2]. Check removal with an iodine spot test across the fabric and a weight-loss test.

Why size must come out

  • Dyeing and bleaching: residual size blocks penetration, giving uneven or pale shades [1][2].
  • Handle: if finishing is wrong, partial desizing and re-finishing may be used to correct the handle [2, p. 331].
  • Absorbency: goods for towels and similar products need clean, absorbent fibre.

How starch size is removed

Starch must be broken down into dextrins or sugars, which wash out more easily than unchanged starch [2, p. 330]:

Method How it works Notes
Enzymatic (amylase) Enzymes break starch into soluble fragments Preferred by many because they have “no deleterious action on the cloth”; rapid and controllable [2, pp. 330–331]. Most common for cotton [1].
Oxidative (e.g. peroxide, persulphate) Oxidises and solubilises starch Also cleans, but can attack the fibre [1]
Acid steeping Hydrolyses starch Risk of degrading cellulose [1]
Hot water or caustic alone — Less effective on starch sizes [1]. Older tests found long boiling or mild caustic did not remove starch completely [2, p. 331].

What makes desizing harder

From a trade review [1]:

  • size viscosity, film solubility and the amount applied;
  • plasticisers and other additives in the size;
  • fabric construction (tightly woven, heavy goods);
  • enzyme conditions: enzymes work in a narrow pH range, need a stabiliser, and can be “poisoned” by some chemicals;
  • poor wetting, which surfactants help with (non-ionic types are generally suitable).

How to check desizing

  1. Iodine spot test: spot iodine solution at several points across the width (sides and centre) and along the length. A blue or violet colour shows remaining starch [1].
  2. Weight loss: weigh fabric before and after desizing, and compare with a well-desized lab sample [1].
  3. Dye trial: a small dye test on desized fabric shows uneven penetration early.

What the sizing side can do

  • Use the size add-on you need, not more. More size is more to remove.
  • Prefer size films that dissolve and break down readily. Converted starches give lower viscosity at the same solids [2, p. 325].
  • Tell the dye house what is in the size (starch type, PVA, additives), so it can set the desizing recipe.

For the trade-offs between starch and PVA sizes, see starch vs PVA for warp sizing.

FAQ

What is desizing in textiles? Removing the warp size from woven fabric before bleaching, dyeing or printing [2, p. 330].

Why does fabric dye unevenly after weaving? A common cause is incomplete desizing: residual size blocks dye penetration [1][2].

How do I test whether starch size has been removed? Use an iodine spot test across and along the fabric, plus a weight-loss test against a well-desized reference [1].

Choosing a sizing starch? Shalbond makes thin-boiling and oxidised starches for warp sizing in India. Tell us your yarn, size recipe and desizing route, and we will send a lab sample with TDS and COA. Request a sample or message us on WhatsApp at +91 89897 00688.

Need a Specific DE Value
or Compliance Certificate?

Our food science team will match your exact specification and send a 1kg lab sample with full COA within 48 hours. No minimum order for initial qualification.

💬